Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00250 GPa | 0.362 ksi | ASTM D412 |
Advanced Polymer Alloys DuraGrip™ 6140 TR Thermoplastic Elastomer DuraGrip® DGR6140TR is a translucent thermoplastic elastomer formulated for excellent elastic properties and enhanced adhesion to various engineered thermoplastics using insert molding, co-injectio.. |