Mechanical Properties Metric English Comments
300% Modulus 0.00110 GPa
0.160 ksi
Measured on films cast from a solution in toluene; ISO 37
Kraton® D1119 B (SIS) Linear Triblock Copolymer
Description: Kraton D1119 B is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from South America in the physical form identified: ..
300% Modulus 0.00110 GPa
0.160 ksi
Measured on films cast from a solution in toluene; ASTM D412
Kraton® D1119 P (SIS) Linear Triblock Copolymer
Description: Kraton D1119 P is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified: ..