Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Kraton
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kraton® D1119 B (SIS) Linear Triblock Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Kraton D1119 B is a clear, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from South America in the physical form identified: Kraton D1119 BT - supplied as a porous pellet dusted with talcRegion: South America, Europe, Asia Pacific, North America, and Japan Uses: Kraton D1119 B is used as an ingredient in formulating adhesives, sealants and coatings. It may also find use as a modifier of bitumen and polymers.Applications: Adhesives, Sealant and Coatings; Compounding and Personal Hygiene; Impact Modification; Footwear; and Bitumen ModificationInformation provided by Kraton®
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ISO 2781
Volatiles <= 0.50 %
<= 0.50 %
KM 04
Melt Flow 25 g/10 min

@Load 5.00 kg,
Temperature 200 °C
25 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Ash 0.40 - 0.80 %
0.40 - 0.80 %
Talc; BAM 908
Mechanical Properties Metric English Comments
Hardness, Shore A 30

@Time 30.0 sec
30

@Time 0.00833 hour
Typical values on polymer compression molded at 300°F; ISO 868
Tensile Strength 2.40 MPa
348 psi
Measured on compression molded slabs; ISO 37
Elongation at Break 1000 %
1000 %
Measured on films cast from a solution in toluene; ISO 37
300% Modulus 0.00110 GPa
0.160 ksi
Measured on films cast from a solution in toluene; ISO 37
Chemical Properties Metric English Comments
Diblock Content 66 %
66 %
Descriptive Properties Value Comments
Content Antioxidant
0.1-0.2%, KM 08
Polystyrene
20.5-23.5%, KM 03
Total Extractables
<1.0%, KM 05