Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00103 GPa | 0.150 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2825E Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00103 GPa | 0.150 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2830M Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00103 GPa | 0.150 ksi | ASTM D 412 |
CPT C-Flex® R70-116 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |