Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00103 GPa | 0.149 ksi | Transverse Direction; Injection molded sample tested at 10 in/min with Die D; ASTM D412 |
Kraton® D2104 DI-N (SBS) Compound Description: Kraton D2104 DI-N is an easy processing, general purpose material designed for a wide variety of applications. It is supplied from North America in the physical form identified: D2104 D.. |
|||
300% Modulus | 0.00103 GPa | 0.149 ksi | Typical properties based on film cast from toluene solution.; ASTM D412 |
Kraton® D4150 K (SBS) Linear Block Copolymer Description: Kraton D4150 K is a linear triblock copolymer based on styrene and butadiene with a polystyrene content of 31%. It is supplied from North America in the physical form identified: Kraton.. |
|||
300% Modulus | 0.00103 GPa | 0.149 ksi | Measured on films cast from a solution in toluene; ASTM D412 |
Kraton® D4433 P (O/E SIS) Linear Triblock Copolymer Description: Kraton D4433 P is an oiled, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified:.. |
|||
300% Modulus | 0.00103 GPa | 0.149 ksi | Typical properties based on film cast from toluene solution.; ASTM D412 |
Kraton® D4433 P (SIS) Linear Block Copolymer Description: Kraton D4433 P is an oiled, linear triblock copolymer based on styrene and isoprene with a polystyrene content of 22%. It is supplied from North America in the physical form identified:.. |
|||
300% Modulus | 0.00103 GPa | 0.150 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2825E Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00103 GPa | 0.150 ksi | ASTM D412 |
Teknor Apex MONPRENE® MP 2830M Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
300% Modulus | 0.00103 GPa | 0.150 ksi | ASTM D 412 |
CPT C-Flex® R70-116 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |