Polymer Property : 300% Modulus = 0.0427 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.000294 GPa
0.0427 ksi
JIS K6301
Stellarchem GP-915UB TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..
300% Modulus 0.000294 GPa
0.0427 ksi
JIS K6301
Stellarchem MP-835B TPE Compound
This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete..