Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0414 GPa
6.00 ksi
ASTM D412
SK Chemicals SKYTHANE® S160D Polyester Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
300% Modulus 0.0414 GPa
6.00 ksi
ASTM D412
Lubrizol Estane® ALR E60D Thermoplastic Polyurethane
Type: Estane® ALR E60D is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor..