Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0318 GPa | 4.61 ksi | ISO 37 |
Lubrizol ESTANE® 58144 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |