Lubrizol ESTANE® 58144 Ether Based Thermoplastic Polyurethane (European Grade)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Ether Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 58144 Ether Based Thermoplastic Polyurethane (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible thermoplastic elastomer system that is easy to process in a wide range of equipment. The Estane® TPU portfolio of products offers high performance polyester - and polyether - based resins and compounds in a broad range of hardnesses to meet a variety of application needs.Benefits of Estane® TPU: Outstanding Abrasion and Wear ResistanceExcellent Low Temperature FlexibilitySuperior Toughness and DurabilityEase of Processing and Manufacturing FlexibilityColorability and Paintability with no adhesion promoterApplications: Film & SheetFabric coating & melt coatingWire & CableHose, Tube & ProfileCustom moldingCustom compoundingAutomotive interior/chassis and exterior painted trimInformation provided by Noveon, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ISO 868
Tensile Strength, Ultimate 44.0 MPa
6380 psi
ISO 37
Elongation at Break 410 %
410 %
ISO 37
Tensile Modulus 0.210 GPa
30.5 ksi
ISO 527
50% Modulus 0.0175 GPa
2.54 ksi
ISO 37
100% Modulus 0.0201 GPa
2.92 ksi
ISO 37
300% Modulus 0.0318 GPa
4.61 ksi
ISO 37
Rebound 34 %
34 %
ISO 4662
Tear Strength 160 kN/m
913 pli
with incision; ISO 34B
Abrasion 50
50
mm<sup>3</sup>; ISO 4649
Compression Set 36 %
36 %
70 hrs./22°C; ISO 815
60 %
60 %
24 hrs./70°C; ISO 815
Thermal Properties Metric English Comments
Vicat Softening Point 105 °C
221 °F
A50; ISO 306