Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.0230 GPa | 3.34 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-7185 Polycaprolactone Based TPU Higher mechanical strength, good hydrolytic stability & chemical resistance, weather resistance, heat & fungus resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
300% Modulus | 0.0230 GPa | 3.34 ksi | ISO 37 |
Lubrizol ESTANE® 58149 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |