300% Modulus 0.0120 - 0.0170 GPa
1.74 - 2.47 ksi
35'/145°C; ASTM D412
SYNTHOS Kralex® 1712 Styrene Butadiene Rubber
KRALEX® 1712 is a standard grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 23.5..
300% Modulus 0.0120 - 0.0170 GPa
1.74 - 2.47 ksi
35'/145°C; ASTM D412
SYNTHOS Kralex® 1723 Styrene Butadiene Rubber
KRALEX® 1723 is a Specific grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 23.5..
300% Modulus 0.0120 - 0.0170 GPa
1.74 - 2.47 ksi
35'/145°C; ASTM D412
SYNTHOS Kralex® 1778 Styrene Butadiene Rubber
KRALEX® 1778 is a Specific grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 23.5..