Material Notes:
KRALEX® 1778 is a Specific grade of oil extended styrene butadiene rubber. It is produced by a technology of cold emulsion polymerisation based on soaps of rosin and fatty acids and contains 23.5% of chemically bounded styrene. It is coagulated by a system of acid and organic coagulant, contains 27% (37.5 PHR) of naphthenic extender oil and is stabilized by a non-staining antioxidant.KRALEX® 1778 is appropriate for rubber compounds used in the production of floor coverings, footwear, bicycle tires, articles from foam rubber and various rubber articles having light color shades.It is not approved for production of rubber articles coming into contact with foods or drinking water.Synthos was formerly known as Kaucuk. All information provided by Synthos.
Physical Properties Metric English Comments
Volatiles <= 0.75 %
<= 0.75 %
ASTM D5668
Mooney Viscosity 35 - 47

@Temperature 100 °C
35 - 47

@Temperature 212 °F
(15-1.5 min); ASTM D3346
42 - 54

@Temperature 100 °C
42 - 54

@Temperature 212 °F
(1+4); ASTM D1646
Ash <= 0.40 %
<= 0.40 %
ASTM D5667
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 18.5 MPa
2680 psi
35'/145°C; ASTM D412
Elongation at Break 350 %
350 %
35'/145°C; ASTM D412
300% Modulus 0.0120 - 0.0170 GPa
1.74 - 2.47 ksi
35'/145°C; ASTM D412
Chemical Properties Metric English Comments
Acid Value 3.5 - 6.5
3.5 - 6.5
ASTM D5774
Styrene Content 23.5 %
23.5 %
ASTM D5775
Descriptive Properties Value Comments
50% of Vulcanization t' 50 (min.) 6-10
ASTM D5289
Antioxidant Grade Non-Staining
Compound Safety ts 1 (min.) 2-3.8
ASTM D5289
Ethanol-toluene Extract (%) 29-35
ASTM D5774
Extender Oil Content (%) 27
Extender Oil Grade NAPHTEN
Maximal Moment (dNm) 15-17.5
ASTM D5289
Minimal Moment (dNm) 1.9-2.5
ASTM D5289
Optimal Vulcanization t' 90 (min.) 11-15
ASTM D5289
Soaps content (%) <= 0.3