Mechanical Properties Metric English Comments
300% Modulus 0.0137 GPa
1.98 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR MBT
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
300% Modulus 0.0137 GPa
1.99 ksi
150°C, 40 min., Pressure Vulcanization. 35% Change after 100°C, 70 hrs, Oil Immersion
KKPC KOSYN KNB 35L Acrylonitrile Butadiene Rubber (NBR)
Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. ..
300% Modulus 0.0137 GPa
1.99 ksi
Taiwan PU Corporation TPUI-H90 High Hydrolysis Resistance, Injection Molding Polyether Base TPU
Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Injection MoldingInformation provided by Taiwan PU Corporation.
300% Modulus 0.0137 GPa
1.99 ksi
Taiwan PU Corporation TPUI-T85 Transparent Grade, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), Transparent Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
300% Modulus 0.0137 GPa
1.99 ksi
Taiwan Sheen Soon Sheenthane® A8210F Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD.
300% Modulus 0.0137 GPa
1.99 ksi
Taiwan Sheen Soon Sheenthane® A9050 Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD.
300% Modulus 0.0137 GPa
1.99 ksi
Taiwan Sheen Soon Sheenthane® A9312R Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD.
300% Modulus 0.0137 GPa
1.98 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 1.0 PHR MBT
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
300% Modulus 0.0137 GPa
1.99 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR MBTS
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
300% Modulus 0.0137 GPa
1.99 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 2.0 PHR MBTS
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..