Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Taiwan PU Corporation TPUI-H90 High Hydrolysis Resistance, Injection Molding Polyether Base TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Taiwan PU Corporation
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation TPUI-H90 High Hydrolysis Resistance, Injection Molding Polyether Base TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Injection MoldingInformation provided by Taiwan PU Corporation.
Mechanical Properties Metric English Comments
Hardness, Shore A 90
90
Tensile Strength at Break 39.23 MPa
5690 psi
Elongation at Break 550 %
550 %
100% Modulus 0.00830 GPa
1.20 ksi
300% Modulus 0.0137 GPa
1.99 ksi
Resilience 50
50
%, Impact Resilience
Taber Abrasion, mg/1000 Cycles 25
25
Processing Properties Metric English Comments
Feed Temperature 180 °C
356 °F
Middle Barrel Temperature 185 °C
365 °F
Compress zone
Front Barrel Temperature 190 °C
374 °F
Metering zone
Adapter Temperature 195 °C
383 °F
Die Temperature 195 °C
383 °F
Users viewing this material also viewed the following: