Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.01002 GPa | 1.453 ksi | ISO 527-2/5A/500 |
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer Type : Pearlthane® CLEAR 15N85 is a polyether copolymer-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Outstanding colour, a very low yellowness index as.. |
|||
300% Modulus | 0.01002 GPa | 1.453 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLCOAT® 162K Thermoplastic Polyurethane Elastomer PEARLCOAT® 162K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE.. |