Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Lubrizol Advanced Materials Manufacturing S. S.L. (Former Merquinsa)
Trade Name Pearlthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type : Pearlthane® CLEAR 15N85 is a polyether copolymer-based thermoplastic polyurethane.Main Application : Injection MouldingSpecial Features : Outstanding colour, a very low yellowness index as well as unique transparancy.All information provided by Merquinsa
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ISO 2781
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
ISO 868
Tensile Strength, Yield 35.00 MPa
5076 psi
ISO 527-2/5A/500
Elongation at Break 660 %
660 %
ISO 527-2/5A/500
50% Modulus 0.00500 GPa
0.725 ksi
ISO 527-2/5A/500
100% Modulus 0.00601 GPa
0.872 ksi
ISO 527-2/5A/500
300% Modulus 0.01002 GPa
1.453 ksi
ISO 527-2/5A/500
Tear Strength 95.0 kN/m
542 pli
ISO 34-1B
Abrasion 20
20
loss (mm³); ISO 4649-A
Thermal Properties Metric English Comments
Vicat Softening Point 84.0 °C
183 °F
ISO 306
Processing Properties Metric English Comments
Feed Temperature 40.0 °C
104 °F
Nozzle Temperature 200 - 220 °C
392 - 428 °F
Zone 1 185 - 200 °C
365 - 392 °F
Zone 2 200 - 230 °C
392 - 446 °F
Zone 3 210 - 230 °C
410 - 446 °F
Zone 4 200 - 220 °C
392 - 428 °F
Dry Time 3.00 hour

@Temperature 100 °C
3.00 hour

@Temperature 212 °F
Descriptive Properties Value Comments
Compression Zone 200°C
Metering Zone 195°C