Mechanical Properties Metric English Comments
300% Modulus 0.00230 GPa
0.334 ksi
press cure 11 min./160ºC
TSE Industries Millathane® 26 Millable Polyether Urethane for Food Contact Applications
Millathane 26 is a polyether polyurethane rubber compliant with the United States Code of Federal Regulations*, Title 21 parts 177.1680 and 177.2600. This polyurethane rubber is designed for food co..
300% Modulus 0.00230 GPa
0.334 ksi
press cure 11 min./160ºC
TSE Industries Millathane® 26 Millable Polyether Urethane for Food Contact Applications
Millathane 26 is a polyether polyurethane rubber compliant with the United States Code of Federal Regulations*, Title 21 parts 177.1680 and 177.2600. This polyurethane rubber is designed for food co..
300% Modulus 0.00230 GPa
0.334 ksi
ASTM D638
ELASTO UK Mediprene™ 500520M TPE, Medical Applications, 52A Hardness
All Mediprene™ compounds are designed and manufactured for use in medical and pharmaceutical applications. In both medical and food contact areas, high application demands are found, such as:Low e..
300% Modulus 0.00230 GPa
0.334 ksi
ASTM D 638
API Megol AM DP2392/40 SEBS Adhesion Modified Overmolding for Polar Polymers
Over-molding allows for the creation of composite finished products in a single phase, removing the need for successive gluing or mechanical fixing steps. This also reduces environmental impact as ..