Mechanical Properties Metric English Comments
Adhesive Bond Strength 8.62 MPa

@Thickness 12.7 mm
1250 psi

@Thickness 0.500 in
ASTM D229
Haysite H722 Polyester, Glass Reinforced
H722 is an all-purpose GPO-1 fiberglass mat reinforced thermoset polyester molded sheet. Available in thicknesses ranging from .031" - 2.00". Standard color - Natural. Meets Gov't Specs - LP-509, ..
Adhesive Bond Strength 8.62 MPa
1250 psi
Lap shear, alum to alum, 24 hrs @ 25°C
Tra-Con Tra-Cast 3108 General Purpose Epoxy Casting Compound
TRA-CAST 3108 is a low viscosity two-part formulation recommended for underfill and encapsulating applications where the combination of good mechanical thermal and electrical properties are required..
Adhesive Bond Strength 8.62 MPa
1250 psi
Lap shear, alum to alum, 24 hrs @ 25°C
Tra-Con Tra-Cast 3156 General Purpose Epoxy Casting System
TRA-CAST 3156 is an easy-to-use, low cost, versatile epoxy resin and hardener system developed for general purpose casting applications. It develops excellent adhesion to most metals, plastics, and ..
Adhesive Bond Strength 8.62 MPa
1250 psi
Lap shear, alum to alum, 2 hrs @ 65°C
Tra-Con Tra-Duct 916D01 Electrically Conductive Silver-Filled Epoxy
TRA-DUCT 916D01 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical pr..