Tra-Con Tra-Duct 916D01 Electrically Conductive Silver-Filled Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Electrically Conductive , Filled/Reinforced Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Duct
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Duct 916D01 Electrically Conductive Silver-Filled Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-DUCT 916D01 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical properties. This two-part, smooth paste formulation of refined pure silver and epoxy is free of solvents and copper or carbon additives. It develops strong, durable, electrically and thermally conducting bonds and coatings between many different and dissimilar materials such as metals, ceramics, glass and plastic laminates.. TRA-DUCT 916D01 cures at room temperature and can be sued as a "cold-solder" for heat-sensitive components where hot-soldering is impractical. It also can be used for the assembly and repair of electrical modules, printed circuits, wave guides, flat cable and high frequency shields. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 27000 cP

@Temperature 25.0 °C
27000 cP

@Temperature 77.0 °F
Mixed (cp #52, 10 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
2 hrs @ 65°C
Adhesive Bond Strength 5.52 MPa
800 psi
Lap shear, alum to alum, 24 hrs @ 25°C
8.62 MPa
1250 psi
Lap shear, alum to alum, 2 hrs @ 65°C
9.31 MPa
1350 psi
Lap shear, alum to alum, 1 hr @ 110°C
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 65.0 °C
149 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 0.00090 ohm-cm
0.00090 ohm-cm
cured 2 hrs @ 65°C
Processing Properties Metric English Comments
Cure Time 60.0 - 240 min

@Temperature 65.0 °C
1.00 - 4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30 min
30 min
Descriptive Properties Value Comments
Color Silver
Thixotropic Index 3.3
1 rpm/10 rpm