Polymer Property : Adhesive Bond Strength = 3850 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 26.5 MPa
3850 psi
Lap shear, alum to alum, 1 hr @ 65°C
Tra-Con Tra-Bond 516H03 Blush-Free Epoxy Adhesive
TRA-BOND 516H03 is a modified version of F114 yielding a higher viscosity and lower coefficient of thermal expansion. Information provided by Tra-Con Inc.