Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 16.0 - 20.0 MPa | 2320 - 2900 psi | Steel, Shear; ISO 4587 |
Permabond 2050 Cyanoacrylate, flexible PERMABOND® 2050 is a flexible cyanoacrylate adhesive, exhibiting improved peel strengths when compared to other grades. It has excellent impact and vibration resistance, and is suitable for bonding.. |
|||
Adhesive Bond Strength | 16.0 - 20.0 MPa | 2320 - 2900 psi | Steel, Shear; ISO 4587 |
Permabond 940 Cyanoacrylate, low odor PERMABOND 940 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | 10.0 - 20.0 MPa | 1450 - 2900 psi | steel collar and pin shear; ISO 10123 |
Permabond HL126 Anaerobic Threadlocker PERMABOND® HL126 Threadlocker is a water thin product for locking pre-assembled parts through wicking action. PERMABOND® HL126 Threadlocker prevents vibration loosening. Because of the low viscosi.. |
|||
Adhesive Bond Strength | 14.0 - 20.0 MPa | 2030 - 2900 psi | Mild steel, Shear |
Permabond TA437 Toughened Acrylic Adhesive PERMABOND TA437 is a single component structural acrylic adhesive designed primarily for bonding metals, ferrites and ceramics. The typical fixture time of TA437 when used with Initiator 41 is 30 –.. |
|||
Adhesive Bond Strength | 15.0 - 20.0 MPa | 2180 - 2900 psi | Zinc, Shear |
Permabond TA4592 Toughened Acrylic Adhesive PERMABOND® TA4592 is a two component structural acrylic adhesive ideal for bonding magnets and ferrites for electric motors on fast-moving production lines. Permabond® TA4592 provides high strengt.. |
|||
Adhesive Bond Strength | 17.0 - 20.0 MPa | 2470 - 2900 psi | Zinc, Shear |
Permabond ET538 Epoxy Resin PERMABOND ET538 is a structural, room temperature curing epoxy adhesive that has excellent adhesion to a wide variety of surfaces such as wood, metal, ceramics and many plastic and composite materia.. |
|||
Adhesive Bond Strength | 18.0 - 20.0 MPa | 2610 - 2900 psi | Mild steel, Shear |
Permabond ET538 Epoxy Resin PERMABOND ET538 is a structural, room temperature curing epoxy adhesive that has excellent adhesion to a wide variety of surfaces such as wood, metal, ceramics and many plastic and composite materia.. |
|||
Adhesive Bond Strength | 16.0 - 20.0 MPa | 2320 - 2900 psi | Steel, Shear; ISO 4587 |
Permabond 941 Cyanoacrylate, low odor PERMABOND 941 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | 16.0 - 20.0 MPa | 2320 - 2900 psi | Steel, Shear; ISO 4587 |
Permabond 943 Cyanoacrylate, low odor PERMABOND 943 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | 18.0 - 20.0 MPa | 2610 - 2900 psi | Mild steel, Shear |
Permabond ET514 Epoxy Resin PERMABOND ET514 is a 1:1 mixable epoxy adhesive. It has excellent resistance to impact and vibration and is ideal for structural bonding of metal, wood, composites and certain plastics. Its rapid cu.. |
|||
Adhesive Bond Strength | 16.0 - 20.0 MPa | 2320 - 2900 psi | Steel, Shear; ISO 4587 |
Permabond 947 Cyanoacrylate, low odor PERMABOND 947 is a low odor, non-fogging non-frosting alkoxyethyl cyanoacrylate. The reduced odor improves worker comfort. Unsightly fogging adjacent to bondlines, common with other cyanoacrylate ad.. |
|||
Adhesive Bond Strength | 10.0 - 20.0 MPa | 1450 - 2900 psi | steel collar and pin shear; ISO 10123 |
Permabond A126 Anaerobic Retainer Permabond® A126 is a high-strength anaerobic adhesive for permanent assembly of coaxial assemblies or threaded metal components. The exceptionally low viscosity of this product makes it ideal for u.. |