Mechanical Properties Metric English Comments
Adhesive Bond Strength 18.0 MPa
2610 psi
Tensile Shear Strength; ASTM D1002
Protective Coating PC-SuperEpoxy™ Translucent Epoxy Putty
PC-SUPEREPOXY™ is a non-drip, thixotropic, translucent paste with unlimited uses in bonding, sealing, and as a filler for most materials. Unlike conventional liquid epoxies, PC-SUPEREPOXY™ can be..
Adhesive Bond Strength 18.0 - 22.0 MPa
2610 - 3190 psi
Steel, Shear; ISO 4587
Permabond 105 Cyanoacrylate, for difficult rubbers
PERMABOND® 105 is a low viscosity high purity cyanoacrylate adhesive. It is ideal for use on hard-to-bond plastics and rubbers such as natural rubber, EPDM and butyl rubber. Cyanoacrylate adhesives..
Adhesive Bond Strength 18.0 - 22.0 MPa
2610 - 3190 psi
ISO 4587, Shear
Permabond 790 Cyanoacrylate, Surface insensitive
PERMABOND® 790 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar..
Adhesive Bond Strength 18.0 - 21.0 MPa
2610 - 3050 psi
Mild steel, Shear
Permabond ET505 Epoxy Resin
PERMABOND ET505 is a two-part, 1:1 mixable epoxy adhesive. ET505 is a semi-flexible toughened epoxy adhesive with good adhesion to a variety of substrates such as wood, metal, ceramics and some plas..
Adhesive Bond Strength 18.0 - 22.0 MPa
2610 - 3190 psi
ISO 4587, Shear
Permabond 791 Cyanoacrylate, Surface insensitive
PERMABOND® 791 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar..
Adhesive Bond Strength 18.0 - 22.0 MPa
2610 - 3190 psi
Steel, Shear; ISO 4587
Permabond 795 Cyanoacrylate, Surface insensitive
PERMABOND® 795 is a moderate viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastome..
Adhesive Bond Strength 18.0 - 20.0 MPa
2610 - 2900 psi
Mild steel, Shear
Permabond ET538 Epoxy Resin
PERMABOND ET538 is a structural, room temperature curing epoxy adhesive that has excellent adhesion to a wide variety of surfaces such as wood, metal, ceramics and many plastic and composite materia..
Adhesive Bond Strength 18.0 - 22.0 MPa
2610 - 3190 psi
ISO 4587, Shear
Permabond 792 Cyanoacrylate, Surface insensitive
PERMABOND® 792 is a low viscosity, surface insensitive adhesive that will rapidly bond substrates with acidic surfaces such as wood and plated surfaces. Plastics, metals, ceramics and elastomers ar..
Adhesive Bond Strength 18.0 - 20.0 MPa
2610 - 2900 psi