Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Adhesive Bond Strength = 29.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6003 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6005 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6006 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6007 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6008 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6009 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6010 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6011 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6012 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6013 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6014 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6015 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6809 Adhesive
Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP ..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6813 Adhesive
Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP ..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6001 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6002 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6004 Adhesive
Description: The CYNERGY 6000 SERIES are for use in demanding applications where very fast cure speeds are required. These are single component solvent free materials manufactured in a wide variety..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6801 Adhesive
Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP ..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6802 Adhesive
Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP ..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6803 Adhesive
Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP ..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6804 Adhesive
Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP ..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6805 Adhesive
Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP ..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6806 Adhesive
Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP ..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6807 Adhesive
Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP ..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6808 Adhesive
Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP ..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6810 Adhesive
Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP ..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6811 Adhesive
Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP ..
Adhesive Bond Strength 29.6 MPa
4300 psi
Steel lap shear
Resinlab® CYNERGY CA6812 Adhesive
Description: The CYNERGY 6800 SERIES are clear, high strength products ideal for bonding dissimilar materials with excellent performance on a wide range of surfaces. This series of products has USP ..
Adhesive Bond Strength 29.6 MPa
4300 psi
Lap shear, alum to alum, 15 min @ 90°C
Tra-Con Tra-Bond F112 Fiber Optic Epoxy Adhesive
TRA-BOND F112 is a long pot life, impact resistant, fiber-optic adhesive. This two-part, low viscosity epoxy has the distinct advantage of remaining below 3000 cps for a minimum of 40 minutes. This ..
Adhesive Bond Strength 29.6 MPa
4300 psi
Lap shear, alum to alum, 4 hrs @ 65°C
Tra-Con Tra-Bond 216C04
Information provided by Tra-Con Inc.
Copyright © lookpolymers.com All Rights Reserved