Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 145 MPa @Diameter <=100 mm |
21000 psi @Diameter <=3.94 in |
24hr/23°C/50% RH; IEC 60212-2; IEC/EN 61212-2 5.3 |
Elektro-Isola Etronit IV C Phenolic, Paper Reinforcement, Yellow, Tubes Description: Suitable for electrical and mechanical applications where there is high air humidity. Lowest water absorption of all the Etronit types. Tropical grade. Good electrical properties at hig.. |
|||
Adhesive Bond Strength | 145 MPa @Diameter <=100 mm |
21000 psi @Diameter <=3.94 in |
24hr/23°C/50% RH; IEC 60212-2; IEC/EN 61212-2 5.3 |
Elektro-Isola Etronit IV C S Phenolic, Paper Reinforcement, Black, Tubes Description: Suitable for electrical and mechanical applications where there is high air humidity. Lowest water absorption of all the Etronit types. Tropical grade. Good electrical properties at hig.. |