Mechanical Properties Metric English Comments
Adhesive Bond Strength 8.96 - 15.9 MPa
1300 - 2310 psi
Average value: 11.7 MPa Grade Count:3
Overview of materials for Epoxy Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr..
Adhesive Bond Strength 13.8 - 15.9 MPa

@Temperature -55.0 - 93.0 °C
2000 - 2310 psi

@Temperature -67.0 - 199 °F
Average value: 14.9 MPa Grade Count:1
Overview of materials for Epoxy Molding Compound
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr..