Polymer Property : Tangent Modulus = 931 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tangent Modulus 931 MPa
135000 psi
ASTM D790
Flint Hills AP7535-HS Polypropylene Ultra High Impact Copolymer
Features: Ease of processing, excellent low temperature impact and stiffness.Applications: Injection Molding: Automotive parts, appliances and consumer durablesInformation Provided by Flint Hills Re..