Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tangent Modulus | 931 MPa | 135000 psi | ASTM D790 |
Flint Hills AP7535-HS Polypropylene Ultra High Impact Copolymer Features: Ease of processing, excellent low temperature impact and stiffness.Applications: Injection Molding: Automotive parts, appliances and consumer durablesInformation Provided by Flint Hills Re.. |