Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tangent Modulus | 790 MPa | 115000 psi | ASTM D790 |
Flint Hills P5M4R-034 Polypropylene Random Copolymer Features: Radiation resistant. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: medical devicesInformation Provided by Flint Hills Resources |