Polymer Property : Tangent Modulus = 740 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tangent Modulus 740 MPa
107000 psi
ASTM D790
Flint Hills P6E2A-005B Polypropylene Impact Copolymer
Features: Ultra high impact strength and long term heat aging.Applications: Injection molding and extrusion: high pressure resistance, film and flexible profilesInformation Provided by Flint Hills R..
Tangent Modulus 740 - 1590 MPa
107000 - 230000 psi
Average value: 1250 MPa Grade Count:10
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..