Tangent Modulus 740 - 1590 MPa
107000 - 230000 psi
Average value: 1250 MPa Grade Count:10
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..