Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tangent Modulus | 1240 MPa | 180000 psi | ASTM D790 |
Flint Hills P9G1Z-047 Polypropylene Features: Processing stability. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion: Thick sheetingInformation Provided by Flint Hills Resources |
|||
Tangent Modulus | 1240 - 1620 MPa | 180000 - 235000 psi | Average value: 1370 MPa Grade Count:4 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |