Polymer Property : Tangent Modulus = 1240 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tangent Modulus 1240 MPa
180000 psi
ASTM D790
Flint Hills P9G1Z-047 Polypropylene
Features: Processing stability. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion: Thick sheetingInformation Provided by Flint Hills Resources
Tangent Modulus 1240 - 1620 MPa
180000 - 235000 psi
Average value: 1370 MPa Grade Count:4
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..