Mechanical Properties Metric English Comments
2% Secant Modulus 0.310 GPa
45.0 ksi
12.7mm/min; ASTM D790
Westlake EC1924AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC1924 is a resin that is widely used in the boardstock coating industry. This material has an excellent combination of low neck-in, ease of processing, good chill-..