Material Notes:
WESTLAKE low-density polyethylene EC1924 is a resin that is widely used in the boardstock coating industry. This material has an excellent combination of low neck-in, ease of processing, good chill-roll release, low coefficient of friction (COF) (for ease of indexing carton blanks) and good heat sealability. It is characterized by high-speed processability, excellent drawdown and reliable lot-to-lot consistency.Application/UsesFood-contact applicationsPhotographic paperFDA: This material complies with FDA regulations in 21 CFR, section 177.1520. Kosher Compliant.All information provided by Westlake Chemical
Physical Properties Metric English Comments
Density 0.923 g/cc
0.0333 lb/in³
ASTM D1505
Melt Flow 4.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 10.0 MPa
1450 psi
500mm/min; ASTM D638 Type IV Specimen
Elongation at Break 100 %
100 %
500mm/min; ASTM D638 Type IV Specimen
2% Secant Modulus 0.310 GPa
45.0 ksi
12.7mm/min; ASTM D790
Processing Properties Metric English Comments
Melt Temperature 149 - 166 °C
300 - 330 °F
Descriptive Properties Value Comments
Process Coating
Region US & Canada