Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 1.36 GPa | 197 ksi | ASTM D790 |
Braskem BU004 Blow Molding High Density Polyethylene Containers for lubricating oils, alcohol, cosmetics and yots; Toys.Information provided by Braskem. |