Braskem BU004 Blow Molding High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem BU004 Blow Molding High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Containers for lubricating oils, alcohol, cosmetics and yots; Toys.Information provided by Braskem.
Physical Properties Metric English Comments
Specific Gravity 0.966 g/cc
0.966 g/cc
ASTM D1505/D792
ESCR 100% Igepal® 32 hour

@Temperature 50.0 °C
32 hour

@Temperature 122 °F
h/50%f; compression molded 2 mm notched-plaques; ASTM D1683
ESCR 10% Igepal® 23 hour

@Temperature 50.0 °C
23 hour

@Temperature 122 °F
h/50%f; compression molded 2 mm notched-plaques; ASTM D1683
Melt Flow 0.38 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.38 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
32 g/10 min

@Load 21.6 kg,
Temperature 190 °C
32 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength at Break 29.0 MPa
4210 psi
ASTM D638
Tensile Strength, Yield 33.0 MPa
4790 psi
ASTM D638
2% Secant Modulus 1.36 GPa
197 ksi
ASTM D790
Izod Impact, Notched 3.00 J/cm
5.62 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 79.0 °C
174 °F
ASTM D648
Vicat Softening Point 129 °C
264 °F
ASTM D1525