Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.793 GPa | 115 ksi | ASTM D638 |
CPC - Vycom HITEC® Pipe Grade HDPE High Density Polyethylene Hitec pipe grade HDPE is a special formulation that has high impact strength, and environmental stress crack resistance. Hitec Pipe grade meets Federal specification L-P 390C, ASTM D1248 Type III we.. |