Polymer Property : 2% Secant Modulus = 10.28 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
2% Secant Modulus 0.07088 GPa
10.28 ksi
ASTM D790
Dow AFFINITY™ SM 1300G Polyolefin Plastomer (POP)
AFFINITY™ SM 1300G is an ethylene alpha-olefin resin for Injection Molding is produced via INSITE™ Technology from Dow Plastics. The resin offers excellent performance in durable injection molded..