Mechanical Properties Metric English Comments
2% Secant Modulus 0.758 GPa
110 ksi
Crosshead speed - 0.5" min; ASTM D790
LyondellBasell Alathon® M4661 High Density Polyethylene
ApplicationsALATHON M 4661, formerly known as LYHD 060, exhibits excellent impact, warp and environmental stress crack resistance. Typical applications are closures, institutional seating and consum..