Polymer Property : 2% Secant Modulus = 0.350 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
2% Secant Modulus 0.350 GPa
50.8 ksi
500mm/min; ASTM D638
LG Chemical SEETEC ES440 Ethylene Vinyl Acetate
Characteristics: Good Mechanical Properties and Good Optical PropertiesApplications: Agricultural Film, Shoe solesCSA No. 24937-78-8Information provided by LG Chemical