Mechanical Properties | Metric | English | Comments |
---|---|---|---|
2% Secant Modulus | 0.317 GPa | 46.0 ksi | 0.5"/min; ASTM D790 |
LyondellBasell Petrothene® GA564189 Linear Low Density Polyethylene, Injection Molding Grade PETROTHENE GA564189 exhibits good stiffness and low temperature toughness. Typical applications include trash cans, industrial containers, housewares and toys. Regulatory Status: GA564189 meets the .. |