Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 130 J | 95.9 ft-lb | V-notch |
Carpenter Pyrowear® 53 Tool Steel, Core Tensile Properties Data provided by Carpenter Technology Corporation.This is a carburizing steel possessing good temper resistance and high case hot hardness while maintaining high core impact strength and fracture to.. |