Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 11.5 J | 8.50 ft-lb | V-Notch, Transverse |
International Mold Steel NAK80 Precipitation Hardened Mold Steel Description: NAK80 is a precipitation or age-hardened mold steel with a uniform through hardness of approximately 40 HRc. It is super clean, Vacuum-Arc Remelted steel with uniform grain structure, u.. |
|||
Charpy Impact | 11.5 J | 8.50 ft-lb | V-Notch; Air Cooled from 996°C; 550°C Temper Temperature |
Latrobe LSS™ MGR™ Tool Steel (ASTM A8) TLS MGR tool steel is an air-hardening tool steel that is characterized by a combination of very good toughness, intermediate wear resistance, and excellent dimensional stability in heat treatment. .. |