Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 71.0 J | 52.4 ft-lb | V-Notch, Transverse |
Latrobe Lescalloy® AF 1410 VIM-VAR ; 17 in High Strength Alloy Steel LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical,.. |
|||
Charpy Impact | 71.0 J | 52.4 ft-lb | V-Notch, Transverse |
Latrobe Lescalloy® AF 1410 VIM-VAR ; 9 in High Strength Alloy Steel LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a
variety of critical,.. |