Mechanical Properties Metric English Comments
Charpy Impact 71.0 J
52.4 ft-lb
V-Notch, Transverse
Latrobe Lescalloy® AF 1410 VIM-VAR ; 17 in High Strength Alloy Steel
LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a variety of critical,..
Charpy Impact 71.0 J
52.4 ft-lb
V-Notch, Transverse
Latrobe Lescalloy® AF 1410 VIM-VAR ; 9 in High Strength Alloy Steel
LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a variety of critical,..