Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 55.0 J | 40.6 ft-lb | V notch. Short transverse direction. 200°C tempering temperature (2 + 2h). |
Assab Steels DIEVAR Hot Work Steel DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i.. |
|||
Charpy Impact | 55.0 J @Temperature 100 °C |
40.6 ft-lb @Temperature 212 °F |
V-notch. Short transverse direction. 45 HRC |
Assab Steels DIEVAR Hot Work Steel DIEVAR is a high performance chromium-molybdenum-vanadium alloyed hot work tool steel which offers a very good resistance to heat checking, gross checking, hot wear and plastic deformation. DIEVAR i.. |
|||
Charpy Impact | 55.0 J | 40.6 ft-lb | Longitudinal, (10mmx10mm) |
Bisalloy Steels BisPlate 400 Thickness >80-100 mm A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Dump Truck Wear Liners, Screw Conveyors, Chutes, Storage Bins, Ea.. |
|||
Charpy Impact | 55.0 J | 40.6 ft-lb | Longitudinal, (10mmx10mm) |
Bisalloy Steels BisPlate 400 Thickness 5 - A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Dump Truck Wear Liners, Screw Conveyors, Chutes, Storage Bins, Ea.. |
|||
Charpy Impact | 55.0 J @Temperature -20.0 °C |
40.6 ft-lb @Temperature -4.00 °F |
Transverse |
Bisalloy Steels BisPlate 80PV Thickness >80-100 mm A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.Applications: Transport Road Tankers, Storage .. |
|||
Charpy Impact | 55.0 J @Temperature -20.0 °C |
40.6 ft-lb @Temperature -4.00 °F |
Transverse |
Bisalloy Steels BisPlate 80PV Thickness 6- A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.Applications: Transport Road Tankers, Storage .. |
|||
Charpy Impact | 55.0 J | 40.6 ft-lb | Longitudinal, (10mmx10mm) |
Bisalloy Steels BisPlate 400 Thickness 16-80 mm A through hardened, abrasion resistant steel plate, offering long life expectancy in high impact abrasion applications.Applications: Dump Truck Wear Liners, Screw Conveyors, Chutes, Storage Bins, Ea.. |
|||
Charpy Impact | 55.0 J @Temperature -20.0 °C |
40.6 ft-lb @Temperature -4.00 °F |
Transverse |
Bisalloy Steels BisPlate 80PV Thickness 16-80 mm A high strength steel alternative for designers of unfired pressure vessels that meets the requirements of AS1210 and achieves a light weight structure.Applications: Transport Road Tankers, Storage .. |
|||
Charpy Impact | 55.0 J @Temperature -54.0 °C |
40.6 ft-lb @Temperature -65.2 °F |
V-notch |
Carpenter Pyrowear® 53 Tool Steel, Core Tensile Properties Data provided by Carpenter Technology Corporation.This is a carburizing steel possessing good temper resistance and high case hot hardness while maintaining high core impact strength and fracture to.. |