Polymer Property : Charpy Impact = 37.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 37.0 J
27.3 ft-lb
aged 1000 hours at 760°C (1400°F)
Haynes HR-160® alloy, plate, aged 1000 hours at 760°C (1400°F)
Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an..
Charpy Impact 37.0 J
27.3 ft-lb
Austenitizing Temperature- 1175°C; Tempering Temperature- 565°C
Crucible Steel PM M2 Tool Steel
PM M2 is an improved quality tool steel compared to conventionally produced material. The powder metallurgy process results in a homogeneous microstructure exhibiting a uniform distribution of fine ..