Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 37.0 J | 27.3 ft-lb | aged 1000 hours at 760°C (1400°F) |
Haynes HR-160® alloy, plate, aged 1000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Charpy Impact | 37.0 J | 27.3 ft-lb | Austenitizing Temperature- 1175°C; Tempering Temperature- 565°C |
Crucible Steel PM M2 Tool Steel PM M2 is an improved quality tool steel compared to conventionally produced material. The powder metallurgy process results in a homogeneous microstructure exhibiting a uniform distribution of fine .. |