Mechanical Properties Metric English Comments
Charpy Impact 325 J
240 ft-lb
Typical
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel
Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water ..
Charpy Impact 325 J
240 ft-lb
10 mm sample from annealed plate
ATI Allegheny Ludlum AL 276™ Nickel-Base Alloy, UNS N10276
AL 276 alloy is a nickel-chromium-iron-tungsten alloy which is among the most corrosion resistant of alloys currently available. The AL 276 alloy is widely used in the severest environments encount..
Charpy Impact 325 J
240 ft-lb
V-notch
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 0% Cold Work
Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®..