Polymer Property : Charpy Impact = 22.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact 22.0 J
16.2 ft-lb
Typical (Transverse)
Industeel CLC 1.2738 Prehardened Mold Steel (300HB/30HRC) for Thick Sections
Description: CLC 1.2738 is a 300HB (30HRC) pre-hardened grade specially designed for plastic mold industry. Chromium, Molybdenum, Nickel carbon and manganese additions are optimized to have a fully ..
Charpy Impact 22.0 J

@Temperature -40.0 °C
16.2 ft-lb

@Temperature -40.0 °F
ThyssenKrupp XAR® 550 Structural Steel
This Material Specification applies to 4 to 100 mm thick plates of the wear-resistant special structural steel XAR® 550.Application: The steel may be used for wear exposed structures, e.g. excavati..
Charpy Impact 22.0 J

@Temperature -40.0 °C
16.2 ft-lb

@Temperature -40.0 °F
ThyssenKrupp XAR® SUPRA Structural Steel
This Material Specification applies to 4 to 100 mm thick plates of the wear-resistant special structural steel XAR® SUPRA.Application: The steel may be used for wear exposed structures, e.g. excava..
Charpy Impact 22.0 J
16.2 ft-lb
V Notch, when tempered at 1000°F
Carpenter No. 883® Hot Work Die Steel (Red-Tough) (AISI H13)
No. 883 hot work die steel is a 5% chromium hot work tool steel designed particularly for applications requiring extreme toughness combined with good red-hardness. It has given an extra margin of sa..
Charpy Impact 22.0 J

@Temperature -18.0 °C
16.2 ft-lb

@Temperature -0.400 °F
V-notch
Carpenter Custom 450® Stainless Steel, Condition H900 (Age Hardened 482°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..